Sealing Exterior Porcelain

Hello Tile Sages,

We have about 600 SF of Mirage Esprit 24x24 porcelain tile/pavers sand/gravel set on an exterior patio. I'm confused but the supply chain seems to be: Mirage->Belgard-> Belden Brick

The Patio is a small fence-enclosed space so we choose the Crema Luna color which is pretty much white. Like all things pretty much white it gets dirty outdoors. We live on Lake Huron so the "dirt" is mostly bug corpses and their resulting bug juice smear.

The joints between the pavers are 2" wide and planted with ground cover. Therefore regular power-washing to clean is not a viable option as the water and pressure makes a mess of the planted joints.

I want to seal the porcelain pavers. I know i don't "have" to but I want to as I think it will make cleaning easier. Is this assumption correct?

I have scoured this forum and the interweb to no avail. I have called Mirage and all they will say is I don't "have" to seal them and therefore they have no product recommendation.

Is there any downside to sealing? If not what type of sealer?

I have had good luck with SEK SB-5000 on a concrete patio and am thinking this penetrating sealer might be a good bet?

I appreciate your advice in advance!
__________________
Alan
Arg is offline   Reply With Quote
Sponsored Links
Old 09-09-2019, 11:57 AM   #2
fhueston
Registered User
 
Join Date: Jan 2016
Posts: 154
Do not Seal exterior tile

No do not seal here is why. Keep in mind that the following is related to stone but the same applies to other tile types

Stone Impregnating Sealers are not Bullet Proof
By Frederick M. Hueston
I receive several calls a week with questions on the use of impregnating type sealers for use on outdoor stone as well as interior wet areas such as showers, water fountains etc. The question is simple: Should I seal my stone in these conditions. The following article will provide a reason why stone in wet areas should not be sealed.

Before we discuss the reason why we shouldn’t stone in these conditions a few definitions are necessary
Impregnators or penetrating sealers: Impregnators are designed to penetrate below the surface of the stone and deposit solid particles in the pores of the stone or to coat the individual minerals below the surface of the stone. Water, oil and dirt are restricted from entering the stone. Impregnators can be solvent, or water based. Most impregnators are vapor permeable.
Vapor Permeable: breathability, vapor permeability describes a stones ability to allow water vapor to pass through it.

The case for not sealing stone in wet environments
When stone is exposed to unregulated humidity and temperature fluctuations, like it would in an outdoor environment or in a shower the air contains vapor in what we know as humidity. Temperature along with humidity can result in condensation as well.
Most of the impregnators on the market today our breathable. This simple means that the stone will be protected from water entering the pores of the stone in liquid form but will allow water vapor to pass.
In an wet environments vapor can be present for several reason, rain, high humidity, temperature fluctuations, steam etc. Since these impregnators are breathable this vapor can easily penetrate into the stone. One would think that this is a positive. The fact is that once the vapor enters the stone it can condense and become a liquid. Since impregnators protect against water in its liquid phase it becomes trapped within the stones pores and will not escape until it evaporates or in other words turns into a vapor. Once this water becomes trapped it can result in all kinds of problems. Stones with iron content can begin to oxidize, natural salts with in the stone can become dissolved and cause pitting and spalling. Aesthetically the stone will appear darker since it is constantly wet.
This problem is becoming more of an issue with the increase of stone being used in showers and exterior environments. There are currently several people doing experiments demonstrate that sealer in wet environments can cause these issues. I strongly believe that care should be taken when sealing stone in these wet environments.
__________________
Fred
fhueston is offline   Reply With Quote
Reply

Stonetooling.com   Tile-Assn.com   National Gypsum Permabase


Thread Tools Search this Thread
Search this Thread:

Advanced Search

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump

Similar Threads
Thread Thread Starter Forum Replies Last Post
Confused about sealing exterior saltillo michael_l Cleaning, Restoration and Sealing 4 10-21-2012 03:37 PM
Sealing exterior flagstone Bodie Powers Cleaning, Restoration and Sealing 3 06-25-2012 01:09 PM
Exterior Porcelain John K Cleaning, Restoration and Sealing 3 06-23-2008 05:18 AM
Enhancing/Sealing Exterior Brick Monicakm Tile Forum/Advice Board 3 05-18-2007 11:40 PM
exterior grout sealing, whats best? Racerx Professionals' Hangout 1 07-07-2006 07:20 PM


All times are GMT -6. The time now is 12:26 PM.


Sponsors

Powered by vBulletin® Version 3.7.4
Copyright ©2000 - 2019, Jelsoft Enterprises Ltd.
Copyright 2018 John Bridge & Associates, LLC