Quote:
Originally Posted by bc brick john
not recommended but makes a nice mix is 2/3 thirds ardex X5 to a 1/3 magnaflex.
|
Quote:
Originally Posted by bc brick john
i just gave a recommendation just to use it up rather than it be thrown in a land fill
|
The right recommendation would be to use them without mixing them . No need to throw one of them in a land fill , just mix one and use , then mix the other one and use .
The -- not to do -- is to mix both and use the mixture for tile setting.
But let's say John is right , is there any chemical component(s) which interfere with other ones or , is there any chemical --both chemical mortars -- negative or non beneficial reaction ?